Site-Map RNR Web Mail  
| | | |
   
Butyl Reclaimed Rubber Home > Products > Butyl Reclaimed Rubber    
Butyl Reclaimed Rubber
Specification 1. Chemical Properties
   Ash % Max. 15
   Acetone Extract % Max. 20
   RHC By Difference % Min. 50 %
Specification 2. Physical Properties
   Specific Gravity % Max. 1.20
   Tensile Strength MPA Max. 6.86
   Elongation at Break % Min. 450
   Mooney Viscosity ML (1+4) @ 100¡ÆC Max. 80
  => This above spec is our normal standard according JIS & KS standard.
 
Advantage
   Cost down
   Improve die swell
   Faster Mixing Cycle
   Reduction in consumption of electrical power due to nerve of compound & faster mixing cycle
Application
   Inner Tube
   Inner Liner
   Cable for electric
   Electric Equipment ( Refrigerator, Air conditioner, Washing Machine, ETC)

MSDS Sheet

Sorry, currently not available.
If you¡¯d like to get our MSDS, please contact us by E-mail or Telephone. Contact  /  E-mail : kskim@r-rtech.com  /  Tel : 62 - 21 - 897 - 4481 ~ 4
RNR Jl. Inti ll Blok C5 No. 6-7, Hyundai International Industrial Estate, Lippo Cikarang, Bekasi, Indonesia  
All contents ¨Ï copyright 2011 www.r-rtech.com, All rights reserved.